Experimental investigation of a Portevin-Le Chatelier band in NiâCo-based superalloys in relation to γʹ precipitates at 500 â
Liu, Yanke, Cai, Yulong, Tian, Chenggang, Zhang, Guoliang, Han, Guoming, Fu, Shihua, Cui, Chuanyong, Zhang, QingchuanLanguage:
english
Journal:
Journal of Materials Science & Technology
DOI:
10.1016/j.jmst.2020.02.001
Date:
February, 2020
File:
PDF, 1.94 MB
english, 2020