![](/img/cover-not-exists.png)
Fractographic analysis of silicate glasses by computer vision
Ma, Lingyue, Dugnani, RobertoLanguage:
english
Journal:
Journal of the European Ceramic Society
DOI:
10.1016/j.jeurceramsoc.2020.01.065
Date:
January, 2020
File:
PDF, 6.82 MB
english, 2020