Cycle sequence sensitivity of near threshold fatigue under programmed loading â A fractographic study
Sunder, R.Volume:
135
Journal:
International Journal of Fatigue
DOI:
10.1016/j.ijfatigue.2020.105537
Date:
June, 2020
File:
PDF, 4.65 MB
2020