![](/img/cover-not-exists.png)
Elastic modulus and hardness of cubic GaN grown by molecular beam epitaxy obtained by nanoindentation
GarcÃa Hernández, S.A., Compeán GarcÃa, V.D., López Luna, E., Vidal, M.A.Volume:
699
Journal:
Thin Solid Films
DOI:
10.1016/j.tsf.2020.137915
Date:
April, 2020
File:
PDF, 910 KB
2020