![](/img/cover-not-exists.png)
Degradation of the surface layers of superalloys and thermal-fatigue damage to the structural elements of gas-turbine engines
L. V. Kravchuk, R. I. Kuriat, K. P. Buiskikh, S. G. KiselevskayaVolume:
40
Language:
english
Pages:
8
DOI:
10.1007/s11223-008-9068-1
Date:
September, 2008