![](/img/cover-not-exists.png)
Materials science aspects of stress corrosion cracking of Russian pipelines
Kantor, M.M., Sudin, V.V., Solntsev, K.A., Kolesov, S.S., Kizitov, R.V., Laptev, A.B., Polyansky, V.A., Golubev, I.A., Markov, A.A., Groysman, A., Webster, S., Shakhmatov, A.V., Alkhimenko, A.A., BadrVolume:
121
Year:
2019
Language:
english
Journal:
E3S Web of Conferences
DOI:
10.1051/e3sconf/201912104014
File:
PDF, 325 KB