![](/img/cover-not-exists.png)
Titania-Supported Vanadium Oxide Synthesis by Atomic Layer Deposition and Its Application for Low-Temperature Oxidative Dehydrogenation of Propane
Kazerooni, Hossein, Towfighi Darian, Jafar, Mortazavi, Yadollah, Khadadadi, Abbas Ali, Asadi, RezaJournal:
Catalysis Letters
DOI:
10.1007/s10562-020-03189-w
Date:
March, 2020
File: