![](/img/cover-not-exists.png)
Role of carbon in modifying solidification and microstructure of a Ni-based superalloy with high Al and Ti contents
Zhao, Guang-di, Zang, Xi-min, Sun, Wen-ruJournal:
Journal of Iron and Steel Research International
DOI:
10.1007/s42243-020-00408-x
Date:
April, 2020
File:
PDF, 4.75 MB
2020