![](/img/cover-not-exists.png)
Elevated temperature mechanical properties of Inconel 617 surface oxide using nanoindentation
Salari, Sepehr, Rahman, Md Saifur, Polycarpou, Andreas A., Beheshti, AliVolume:
788
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2020.139539
Date:
June, 2020
File:
PDF, 3.33 MB
2020