Study of the heat transfer coefficient of a nickel-based superalloy in the end-quench test with air
Fu, Pei, Zhou, Ping, Zhao, Tian-yang, Song, Yan-po, Huang, Zai-wangVolume:
155
Journal:
International Journal of Thermal Sciences
DOI:
10.1016/j.ijthermalsci.2020.106416
Date:
September, 2020