Wettability and interfacial reactions of a low Hf-containing nickel-based superalloy on Al2O3-based, SiO2-based, ZrSiO4, and CoAl2O4 substrates

Wang, Haiwei, Yang, Jinxia, Meng, Jie, Yang, Yanhong, Zhou, Yizhou