![](/img/cover-not-exists.png)
Study on hole quality and surface quality of micro-drilling nickel-based single-crystal superalloy
Zhou, Yunguang, Li, Hongyang, Ma, Lianjie, Chen, Jingqiang, Tan, Yanqing, Yin, GuoqiangVolume:
42
Journal:
Journal of the Brazilian Society of Mechanical Sciences and Engineering
DOI:
10.1007/s40430-020-02427-x
Date:
June, 2020
File:
PDF, 3.60 MB
2020