Nanoindentation as a strength probe—a study on the hardness dependence of indent size for fine-grained and coarse-grained ferritic steel
Kensuke Miyahara, Saburo Matsuoka, Tohru HayashiVolume:
32
Language:
english
Pages:
8
DOI:
10.1007/s11661-001-1010-0
Date:
March, 2001