![](/img/cover-not-exists.png)
Tensile Properties of Ni-Based Superalloy 720Li: Temperature and Strain Rate Effects
K. Gopinath, A.K. Gogia, S.V. Kamat, R. Balamuralikrishnan, U. RamamurtyVolume:
39
Language:
english
Pages:
11
DOI:
10.1007/s11661-008-9585-3
Date:
October, 2008
File:
PDF, 894 KB
english, 2008