![](/img/cover-not-exists.png)
Evolution of Microstructure and Texture During Hot Compression of a Ni-Fe-Cr Superalloy
S. P. Coryell, K. O. Findley, M. C. Mataya, E. BrownVolume:
43
Langue:
english
Pages:
17
DOI:
10.1007/s11661-011-0889-3
Date:
February, 2012
Fichier:
PDF, 1.76 MB
english, 2012