Evolution of aluminide coating microstructure on nickel-base cast superalloy CM-247 in a single-step high-activity aluminizing process
D. K. Das, S. V. Joshi, Vakil SinghVolume:
29
Language:
english
Pages:
16
DOI:
10.1007/s11661-998-0042-0
Date:
August, 1998
File:
PDF, 3.16 MB
english, 1998