Superior atomic layer deposition of conformal ZnO shell on spherical SiO2 particles for enhanced photocatalytic activity
Ahmad, Waheed, Basit, Muhammad Abdul, Khan, Muhammad Saad, Ali, Ijaz, Park, Tae JooJournal:
Physica E: Low-dimensional Systems and Nanostructures