![](/img/cover-not-exists.png)
Fractographic and Metallographic Study of Spalling Failure of Steel Straightener Rolls
G. Pantazopoulos, A. VazdirvanidisVolume:
8
Language:
english
Pages:
6
DOI:
10.1007/s11668-008-9170-5
Date:
December, 2008
File:
PDF, 699 KB
english, 2008