Effect of Thermal Aging on the Stress Corrosion Cracking Sensitivity of Z3CN20.09M Stainless Steel
Wu, Huan Chun, Ti, Wen Xin, Li, Cheng Tao, Zhu, Ze Jie, Cao, Fa He, Fang, Ke Wei, Zhang, Guo Dong, Xue, FeiVolume:
993
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.993.474
Date:
May, 2020