![](/img/cover-not-exists.png)
An experimental assessment of methods for mitigating plasticity error during nanoindentation with continuous stiffness measurement
Phani, P. Sudharshan, Oliver, W.C., Pharr, G.M.Volume:
194
Journal:
Materials & Design
DOI:
10.1016/j.matdes.2020.108924
Date:
September, 2020
File:
PDF, 3.58 MB
2020