![](/img/cover-not-exists.png)
Galvanic Coupling Effect on Pitting Corrosion of 316L Austenitic Stainless Steel Welded Joints
Sriba, Amina, Vogt, Jean-BernardJournal:
Metals and Materials International
DOI:
10.1007/s12540-020-00789-4
Date:
July, 2020
File:
PDF, 2.05 MB
2020