![](/img/cover-not-exists.png)
Characterization of stress corrosion crack growth of 304 stainless steel by electrochemical noise and scanning Kelvin probe
Ru Zhao, Zheng Zhang, Jiang-bo Shi, Lei Tao, Shi-zhe SongVolume:
17
Language:
english
Pages:
6
DOI:
10.1007/s11771-010-0003-9
Date:
February, 2010
File:
PDF, 1010 KB
english, 2010