Simulation of stray grain formation during unidirectional solidification of IN738LC superalloy
Xiang-mei Li, Jie-yu Zhang, Bo Wang, Zhong-ming Ren, Guo-zhi ZhouVolume:
18
Language:
english
Pages:
6
DOI:
10.1007/s11771-011-0653-2
Date:
February, 2011
File:
PDF, 941 KB