![](/img/cover-not-exists.png)
A freckle criterion for the solidification of superalloys with a tilted solidification front
Wan-Hong Yang, John J. deBarbadillo, Koki Morita, T. Suzuki, Wei Chen, Keh-Minn ChangVolume:
56
Language:
english
Pages:
6
DOI:
10.1007/s11837-004-0202-7
Date:
September, 2004
File:
PDF, 782 KB