![](/img/cover-not-exists.png)
An optimal approach for improving the machinability of Nimonic C-263 superalloy during cryogenic assisted turning
Jadhav, Prashant S., Mohanty, Chinmaya P., Hotta, Tapano Kumar, Gupta, ManojVolume:
58
Journal:
Journal of Manufacturing Processes
DOI:
10.1016/j.jmapro.2020.08.017
Date:
October, 2020
File:
PDF, 2.45 MB
2020