Influences of Cr/Ni equivalent ratios of filler wires on pitting corrosion and ductility-dip cracking of AISI 316L weld metals
Y. H. Kim, D. G. Kim, J. H. Sung, I. S. Kim, D. E. Ko, N. H. Kang, H. U. Hong, J. H. Park, H. W. LeeVolume: