Strength degradation and fractographic analysis of carbon fiber reinforced polymer composite laminates with square / circular hole using scanning electron microscope micrographs
Gupta, Savita, Prusty, Rajesh Kumar, Ray, Bankim Chandra, Pal, SnehanshuJournal:
Journal of Applied Polymer Science
DOI:
10.1002/app.49878
Date:
November, 2020
File:
PDF, 4.36 MB
2020