Influence of the Mechanical Properties of Elastoplastic Materials on the Nanoindentation Loading Response
Yang, Huanping, Zhuang, Wei, Yan, Wenbin, Wang, YaomianVolume:
13
Journal:
Materials
DOI:
10.3390/ma13214842
Date:
October, 2020