Evaluation of susceptibility to stress corrosion cracking based on non-linear eddy current method
Oikawa, Ryota, Uchimoto, Tetsuya, Takagi, Toshiyuki, Urayama, Ryoichi, Nemoto, Yoshiyuki, Takaya, Shigeru, Keyakida, SatoshiVolume:
33
Journal:
International Journal of Applied Electromagnetics and Mechanics
DOI:
10.3233/jae-2010-1254
Date:
October, 2010
File:
PDF, 697 KB
2010