Investigating the stress corrosion cracking of a biodegradable Zn-0.8Â wt%Li alloy in simulated body fluid
Li, Guan-Nan, Zhu, Su-Ming, Nie, Jian-Feng, Zheng, Yufeng, Sun, ZhiliVolume:
6
Journal:
Bioactive Materials
DOI:
10.1016/j.bioactmat.2020.10.009
Date:
May, 2021
File:
PDF, 133 KB
2021