![](/img/cover-not-exists.png)
Free-radical polymerization of lauryl methacrylate by differential scanning calorimetry: Part 1. Enthalpy of polymerization
P.K. Mahato, D. Chanda, A. Borthakur, K.V. RaoVolume:
222
Year:
1993
Language:
english
Pages:
7
DOI:
10.1016/0040-6031(93)80559-s
File:
PDF, 394 KB
english, 1993