![](/img/cover-not-exists.png)
Operating stresses and stress corrosion cracking in steam generator transition zones (900-MWe PWR)
B. Flesch, P. Vidal, J. Chabrerie, J.P. BrunetVolume:
56
Year:
1993
Language:
english
Pages:
16
DOI:
10.1016/0308-0161(93)90094-a
File:
PDF, 691 KB