Modification of interparticle forces for nanoparticles using atomic layer deposition
L.F. Hakim, J.H. Blackson, A.W. WeimerVolume:
62
Year:
2007
Language:
english
Pages:
13
DOI:
10.1016/j.ces.2007.07.013