Research on vacuum-electromagnetic casting of IN100 superalloy ingots
Wenzhong Jin, Tingju Li, Guomao YinVolume:
8
Year:
2007
Language:
english
Pages:
4
DOI:
10.1016/j.stam.2006.12.001
File:
PDF, 408 KB
english, 2007