A Code of Practice for conducting notched bar creep tests and for interpreting the data
G. A. WEBSTER, S. R. HOLDSWORTH, M. S. LOVEDAY, K. NIKBIN, I. J. PERRIN, H. PURPER, R. P. SKELTON, M. W. SPINDLERVolume:
27
Year:
2004
Language:
english
Pages:
24
DOI:
10.1111/j.1460-2695.2004.00765.x
File:
PDF, 435 KB