![](/img/cover-not-exists.png)
X-ray fractography of a diesel engine crankshaft
I. FERNÁNDEZ PARIENTE, M. GUAGLIANOVolume:
31
Year:
2008
Language:
english
Pages:
14
DOI:
10.1111/j.1460-2695.2007.01204.x
File:
PDF, 372 KB
english, 2008