Fractography, Mechanical Properties, and Microstructure of Commercial Silicon Nitride–Titanium Nitride Composites
Gurdial Blugan, Mousab Hadad, Jolanta Janczak-Rusch, Jakob Kuebler, Thomas GrauleVolume:
88
Year:
2005
Language:
english
Pages:
8
DOI:
10.1111/j.1551-2916.2005.00186.x
File:
PDF, 1.26 MB
english, 2005